| 廠家及牌號(hào) | 試驗(yàn)條件 | 測(cè)試方法 | 磨損因數(shù)-Washer |
| PBT 沙伯基礎(chǔ) LNP™ LUBRICOMP™ WAL34 compound | ASTMD3702Modified | 6.00 10^-10in^5-min/ft-lb-hr | |
| PBT 沙伯基礎(chǔ) LNP™ LUBRICOMP™ WFL36 compound | ASTMD3702Modified | 42.0 10^-10in^5-min/ft-lb-hr | |
| PBT 沙伯基礎(chǔ) LNP™ LUBRICOMP™ WFL36E compound | ASTMD3702Modified | 24.0 10^-10in^5-min/ft-lb-hr | |
| PBT 沙伯基礎(chǔ) LNP™ LUBRICOMP™ WL004 compound | ASTMD3702Modified | 58.0 10^-10in^5-min/ft-lb-hr | |
| 該文獻(xiàn)版權(quán)所有-請(qǐng)勿轉(zhuǎn)載或-其它用途.http://www.adultegratos.com/ | |||
| PBT 沙伯基礎(chǔ) LNP™ LUBRICOMP™ WX07423H compound (潤(rùn)滑,注射成型) | ASTMD3702Modified | 5.00 10^-10in^5-min/ft-lb-hr | |
| PBT 沙伯基礎(chǔ) LNP™ LUBRICOMP™ WFL369 compound | ASTMD3702Modified | 25.2 10^-10in^5-min/ft-lb-hr | |
| PBT 沙伯基礎(chǔ) LNP™ LUBRICOMP™ WFP36 compound | ASTMD3702Modified | 136 10^-10in^5-min/ft-lb-hr | |
| PBT 沙伯基礎(chǔ) LNP™ LUBRICOMP™ WBL36L compound | ASTMD3702Modified | 25.0 10^-10in^5-min/ft-lb-hr | |
| PBT 沙伯基礎(chǔ) LNP™ LUBRICOMP™ WFI14 compound (潤(rùn)滑,注射成型填料:玻璃纖維增強(qiáng)材料。) | ASTMD3702Modified | 113 10^-10in^5-min/ft-lb-hr | |
| PBT 沙伯基礎(chǔ) LNP™ LUBRICOMP™ WFL34H compound | ASTMD3702Modified | 35.0 10^-10in^5-min/ft-lb-hr | |
| 溫馨提示 | |||
| 1.有關(guān)“磨損因數(shù)-Washer PBT”類數(shù)據(jù)資訊最多展示10條.更多牌號(hào)應(yīng)用數(shù)據(jù)請(qǐng)向客服索取。 2.有關(guān)“PBT塑料原料”類數(shù)據(jù)的實(shí)時(shí)性及更多塑料原料行情敬請(qǐng)關(guān)注我們的資訊動(dòng)態(tài). | |||
● PC+聚酯 熔流率(熔體流動(dòng)速率)(300°C/1.2kg)
● PPO(PPE)+SEBS 拉伸模量
● PA12 MoldingShrinkage-AcrossFlow(24hr)
● PP共聚 霧度(50.0um)
● AS UL阻燃等級(jí)