| 廠家及牌號(hào) | 試驗(yàn)條件 | 測(cè)試方法 | 吸水率(24hr,50%RH) |
| PA6 沙伯基礎(chǔ) LNP™ LUBRICOMP™ PFL38S compound | ASTMD570 | 0.50 % | |
| PA6 沙伯基礎(chǔ) LNP™ KONDUIT™ PX09322 compound (導(dǎo)熱,阻燃性,注射成型填料:礦物填料。) | ASTMD570 | 0.060 % | |
| PA6 沙伯基礎(chǔ) LNP™ THERMOTUF™ PF006I compound (抗撞擊性高,注射成型填料:玻璃纖維增強(qiáng)材料, 30% 填料按重量。) | ASTMD570 | 0.83 % | |
| PA6 沙伯基礎(chǔ) LNP™ THERMOCOMP™ PF008 compound | ASTMD570 | 0.98 % | |
| 此文獻(xiàn)-版權(quán)所有-請(qǐng)勿轉(zhuǎn)載-或其它用途.http://www.adultegratos.com/ | |||
| PA6 沙伯基礎(chǔ) LNP™ STAT-KON™ PFD06 compound | ASTMD570 | 0.50 % | |
| PA6 沙伯基礎(chǔ) LNP™ THERMOCOMP™ PF006 compound (注射成型填料:玻璃纖維增強(qiáng)材料, 30% 填料按重量。) | ASTMD570 | 0.86 % | |
| PA6 沙伯基礎(chǔ) LNP™ THERMOCOMP™ PF00ASXS compound | ASTMD570 | 0.83 % | |
| PA6 法國(guó)Eurostar Starflam PZ0052E (磷含量低(到無(wú)),阻燃性,無(wú)鹵,注射成型填料:玻璃纖維增強(qiáng)材料。) | ASTMD570 | 1.1 % | |
| PA6 沙伯基礎(chǔ) LNP™ THERMOCOMP™ PF008S compound | ASTMD570 | 0.98 % | |
| PA6 沙伯基礎(chǔ) LNP™ THERMOCOMP™ PX01658 compound (注射成型填料:專有填料。) | ASTMD570 | 0.75 % | |
| 溫馨提示 | |||
| 1.有關(guān)“吸水率(24hr,50%RH) PA6”類數(shù)據(jù)資訊最多展示10條.更多牌號(hào)應(yīng)用數(shù)據(jù)請(qǐng)向客服索取。 2.有關(guān)“PA6塑料原料價(jià)格”類數(shù)據(jù)的實(shí)時(shí)性及更多塑料原料價(jià)格行情敬請(qǐng)關(guān)注我們的資訊動(dòng)態(tài). | |||
● MDPE 脆化溫度
● PVDF 熔點(diǎn)
● PC/ABS TensileStrength(Break,3.20mm,InjectionMolded)
● PUR 抗張強(qiáng)度 (斷裂)
● TPU 拉伸應(yīng)力(斷裂)